Nil Tiritoğlu İnşaat
Detailed Info

Product features & application

  • Cement-based block adhesive mortar with reinforced bonding adherence
  • Reduces thermal bridging at the joints with 0.26 W/mK thermal conductivity
  • Class M10 compressive strength of > 13 N/mm²
  • Tensile adhesion strength of 0.65 N/mm² after water immersion
  • Tensile adhesion strength of 0.59 N/mm² after heat ageing
  • Workability time of 80 ± 5 min
  • Low class W1 water absorption (≤ 0.15 kg/m²·min^0.5)
  • Class A1 non-combustible material
Contact